Full metadata record
DC FieldValueLanguage
dc.contributor.authorЯрмоленко, М.А.-
dc.contributor.authorРогачёв, А.А.-
dc.contributor.authorЛю Имин-
dc.contributor.authorРогачёв, А.В.-
dc.contributor.authorГао Лихун-
dc.contributor.authorМа Чжуа-
dc.contributor.authorYarmolenko, M.A.-
dc.contributor.authorRogachev, A.А.-
dc.contributor.authorYiming Liu-
dc.contributor.authorRogachev, A.V.-
dc.contributor.authorLihong Gao-
dc.contributor.authorZhuang Ma-
dc.date.accessioned2022-03-29T12:50:18Z-
dc.date.available2022-03-29T12:50:18Z-
dc.date.issued2022-
dc.identifier.citationОсобенности деградации полимерных материалов при воздействии коротковолнового лазерного излучения / М.А. Ярмоленко [и др.] // Проблемы физики, математики и техники. Сер.: Физика. - 2022. - № 1 (50). - С. 49-54.ru
dc.identifier.urihttp://elib.gsu.by/jspui/handle/123456789/36082-
dc.description.abstractОпределены особенности деградации высокомолекулярных соединений (кремнийорганическая смола, политетрафторэтилен) их смесей с формиатом меди в условиях воздействия лазерного излучения с различной длиной волны. Проведена оценка реакционной активности генерируемых летучих продуктов деструкции. Исследована молекулярная структура и морфология осаждаемых покрытий. При одинаковой интенсивности воздействие более коротковолнового лазерного излучения (λ = 266 нм) на кремнийорганический полимер приводит к формированию покрытий с меньшей концентрацией Si – O – C групп по отношению к содержанию групп Si – С₆Н₅ в сравнении с излучением с длиной волны 535 и 355 нм. Значение длины лазерного излучения не оказывает заметного влияния на молекулярную структуру покрытий на основе ПТФЭ и ПТФЭ + медь. Это может свидетельствовать о преимущественно фототермическом механизме деградации исходных мишеней. The features of macromolecular compounds (organosilicon resin, polytetrafluoroethylene) of their mixtures with copper formate degradation under the influence of laser radiation with different wavelengths are determined. The reactivity of the generated volatile degradation products was evaluated. The molecular structure and morphology of deposited coatings were studied. At the same intensity, the influence of shorter-wavelength laser radiation (λ = 266 nm) on an organosilicon polymer leads to the formation of coatings with a lower concentration of Si – O – C groups relative to the content of Si – С₆Н₅ groups compared to radiation with a wavelength of 535 and 355 nm. The value of the laser radiation length has no noticeable effect on the molecular structure of coatings based on PTFE and PTFE + copper. This may indicate a predominantly photothermal mechanism of the initial targets degradation.ru
dc.language.isoРусскийru
dc.publisherГомельский государственный университет имени Ф. Скориныru
dc.subjectлазерное диспергированиеru
dc.subjectактивная газовая фазаru
dc.subjectполимерru
dc.subjectкремнийорганикаru
dc.subjectпокрытиеru
dc.subjectметаллru
dc.subjectмолекулярная структураru
dc.subjectaser dispersionru
dc.subjectactive gas phaseru
dc.subjectpolymerru
dc.subjectorganosiliconru
dc.subjectcoatingru
dc.subjectmetalru
dc.subjectmolecular structureru
dc.titleОсобенности деградации полимерных материалов при воздействии коротковолнового лазерного излученияru
dc.title.alternativeFeatures of polymer materials degradation under influence of short-wave laser radiationru
dc.typeArticleru
dc.identifier.udk539.375.5:678.07:544.032.65-
dc.rootПроблемы физики, математики и техникиru
dc.placeOfPublicationГомельru
dc.seriesФизикаru
dc.number1 (50)ru
dc.identifier.DOIhttps://doi.org/10.54341/20778708_2022_1_50_49ru
Appears in Collections:Проблемы физики, математики, техники. Физика

Files in This Item:
File Description SizeFormat 
Ярмоленко_Особенности.pdf600.29 kBAdobe PDFView/Open


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.